-40%
Tanning Bed Acrylic Sunscape 755 Shoulder
$ 335.28
- Description
- Size Guide
Description
BUY WITH CONFIDENCE SINCE 1991SHOULDER ACRYLIC SUNSCAPE 755 TANNING BED
You will need to remove the existing center mounting bracket (4 small screws) and putting our metal bracket in its place, then the shoulder tanner will fit on snuggly and you will just use the one center fastener that we are also providing. ETS when they made these shoulder tanners actually had 3 different versions and had to change their acrylics twice. They decided not to make anymore of these. Our acrylic manufacturer has finally come up with this universal acrylic to work on all 3 styles
.
THERE IS ACTUAL PICTURE OF ACRYLIC AND BRACKET IN PHOTO GALLERY
Shoulder Acrylic (we do have the bottom available)
Free shipping in Continental USA
RIGHT NOW HANDLING TIME IS 5-7 DAYS BECAUSE THEY HAVE JUST STARTED MAKING THESE. ONCE ORDERS ARE CAUGHT UP THE HANDLING TIME WILL BE LESS
LET ME KNOW WHAT YOU NEED AND I WILL GET YOU THE CORRECT ITEM NUMBER TO PURCHASE
WE CARRY ALL BED MANUFACTURERS ACRYLICS
MADE IN THE USA
If this is not what you're looking for please contact me
for the acrylic you need and I will get you the right item number acrylic
CONTACT RONNIE FOR QUESTIONS
LOTION DISCOUNTS FOR TANNING SALONS AND HOME TANNING BED OWNERS
WE ARE A FULL SERVICE TANNING DISTRIBUTOR
ABOUT US:
WE CARRY FULL LINE OF :
NEW AND USED TANNING BEDS
TANNING BED PARTS
TANNING BED ACRYLICS
TANNING LOTIONS
TANNING SUPPLIES FOR THE SALON
SUNLESS TANNING BOOTHS
AIR BRUSH TANNING SYSTEMS
OVER 21 YEARS SERVING THE TANNING INDUSTRY
INDEPENDENT FAMILY OWNED COMPANY
FREE TECHNICAL SUPPORT FOR OUR CUSTOMER
Frequently Asked Questions
Q.
What should I clean my acrylic with.
A.
Only a acrylic cleaner formulated especially for
tanning acrylics should be used. Household cleaners do not have the germ or bacteria killing strength to sanitize your bed. Most household cleaners are often irritating to the skin.
Q.
What can I use to clean off finger nail polish.
A.
You can use lighter fluid or another acetone type
solvent to clean the polish off. Immediately wash the area with bed cleaner to remove all the solvent. If solvent residue remains on the surface, the acrylic may craze.
Q.
How often should I replace my acrylics?
A.
Both acrylics should be replaced every 1500 hours
(2 bulb changes). Although an acrylic may look
clear after 1500 hours the transmission rate of the acrylic has dropped considerable. Why put new bulbs in a bed if the full effect doesn't reach the customer?
Q.
What causes crazing in the bends?
A.
Excessive heat or excessive age usually causes
crazing inside of the bends.
Q.
What causes surface crazing?
A.
Surface crazing usually is a result of a non-
indoor tanning lotions being used or an
improper bed cleaning solution. Since acrylic
is a petroleum based product any products
containing oils will craze the surface.
Q.
Why did my acrylic break or crack?
A.
The Major reasons are:
1. Due to exposure to the radiation an acrylic
only has a life span of about 1500 hours
(2 bulb changes). Excessively high UVB
strength of modern lamps also accelerates
the acrylic premature failure.
2. The bed has been overheating due to
cooling fans out or installed incorrectly
3. Excessive weight on the acrylic. Most
beds will adequately support most
people. However some beds lack an
adequate support system for the acrylic.
Extra supports can be purchased
if an acrylic breakage problem continues.
Q.
What is Annealing?
A.
Annealing is the process of reheating an acrylic to its molding point and then cooling back down. This relieves the stress caused in forming.
Q.
Can I repair a cracked acrylic?
A.
Broken acrylics can not be successfully repaired.
Internet Warning: Beware
of sites selling cheaply made tanning bed acrylics, with limited warranties. Many of these sites use untested foreign made acrylic.
Know your Seller!
Do they have their name and address on their site? Do you really know who they are?
WE WILL EMAIL YOU TO VERIFY THAT THIS IS THE ACRYLIC YOU ARE WANTING TO BE SURE YOU GET THE CORRECT ACRYLIC
We always verify your order so that you are getting the correct acrylic
RETURN POLICY
:
1. We only accept returns if we sent you the wrong acrylic.
2.
If any acrylics are damaged we will replace them and reship replacements at our cost.
3. WE WILL VERIFY YOUR ORDER BEFORE WE SHIP TO BE SURE YOU ARE GETTING WHAT YOU ORDERED
THANK YOU
RONNIE